A Study of the Effect of Magnetic Fields Using Welding Process
Hong Seok Cho, Ik Keun Park, Wooram Lee
J Weld Join. 2014;32(5):462-473.   Published online October 30, 2014
PDFPDF    
2031618
Welding Characteristics of A-TIG Using Various Compositions of Active Fluxes
Bong-Hun Kim, Yong-Soo Gong
J Weld Join. 2014;32(5):456-461.   Published online October 30, 2014
PDFPDF    
2031615
The Effects of Welding Wires on the Weldabilities of API X-100 with Laser-Arc Hybrid Welidng
Sungwook Kim, MOK-Young Lee
J Weld Join. 2014;32(5):437-442.   Published online October 30, 2014
PDFPDF    
2031614
Evaluation of HIC/SSCC Resistance for API-X70 Pipe Manufactured by JCO Bending Process and SA Welding
Hoi-Soo Ryoo, Hee Jin Kim, Dong-Eon Lee
J Weld Join. 2014;32(5):431-436.   Published online October 30, 2014
PDFPDF    
2031602
Numerical Studies on Submerged Arc Welding Process
Degala Ventaka Kiran, Suck-Joo Na
J Weld Join. 2014;32(4):339-347.   Published online August 30, 2014
PDFPDF    
2031591
Plasma Electrolytic Oxidation in Surface Modification of Metals for Electronics
Mukesh Kumar Sharma, Youngjoo Jang, Jongmin Kim, Hyungtae Kim, Jae Pil Jung
J Weld Join. 2014;32(3):241-247.   Published online June 30, 2014
PDFPDF    
2031587
Experimental Studies on Submerged Arc Welding Process
Degala Ventaka Kiran, Suck-Joo Na
J Weld Join. 2014;32(3):215-224.   Published online June 30, 2014
PDFPDF    
2031582
Proper Arc Welding Condition Derivation of Auto-body Steel by Artificial Neural Network
Jungho Cho
J Weld Join. 2014;32(2):169-173.   Published online May 14, 2014
PDFPDF    
2031574
Weldability Increase of Aluminum by Variable Polarity Arc
Jungho Cho
J Weld Join. 2014;32(1):108-111.   Published online February 27, 2014
PDFPDF    
2031552
Development of Welding Quality Monitoring Method for TIG Cladding
Sang Myung Cho, Min Su Son, Jung Hyun, Park
J Weld Join. 2013;31(6):90-95.   Published online January 21, 2014
PDFPDF    
2031558
Porosity Reduction in Laser Welding of Nitrided Carbon Steel
Young-Nam Ahn, Cheolhee Kim, Wonbeom Lee, Jeonhan Kim
J Weld Join. 2013;31(6):71-76.   Published online January 21, 2014
PDFPDF    
2031525
LIBS Analysis on Magnetic Force of Dissimilar Material Using SMAW
Chul Ku Lee, Wooram Lee
J Weld Join. 2013;31(4):54-61.   Published online August 31, 2013
PDFPDF    
2031508
Development of Push-pull Type Arc Welding Wire Feeder
Hyun-Jun Yoon, In-Sung Hwang, Dong-Cheol Kim, Moon-Jin Kang, Ki-Gab Choi
J Weld Join. 2013;31(3):39-43.   Published online July 10, 2013
PDFPDF    
Prediction of Arc Welding Quality through Artificial Neural Network
Jungho Cho
J Weld Join. 2013;31(3):44-48.   Published online June 30, 2013
PDFPDF    
Recent Technological Tendency of Laser/Arc Hybrid Welding
Youngsik Kim, Sangcheol Kil
J Weld Join. 2013;31(2):4-15.   Published online June 5, 2013
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI